Contact
RIBBED SMOKED SHEET CLASSIFICATION (Based on The Green Book, 1969)
| Grade | Rubber Mold | Wrapping mold | Opaque spots | Over smoked spots | Oxidized spots | Burnt sheet |
|---|---|---|---|---|---|---|
| RSS1 | Very slight | Very slight | No | No | No | No |
| RSS2 | Slight | Slight | No | No | No | No |
| RSS3 | Slight | Slight | Slight | No | No | No |
| RSS4 | Slight | Slight | Slight | Slight | No | No |
| RSS5 | Slight | Slight | Slight | Slight | N/A | No |
| Grade | Brief Description of RSS Grades (based on The Green Book-1969) |
|---|---|
| RSS1 | Clean, dry, strong, small-scattered pinhead bubbles, free from blemishes, sand, foreign matter, under-cured |
| RSS2 | Dry mould no more than 5%, clean, dry, strong, small-scattered bubbles, specks of bark, free from blemishes, sand, foreign matter, under-cured. |
| RSS3 | Dry mould no more than 10%, clean , dry, strong, small-scattered bubbles, specks of bark, free from blemishes, sand, foreign matter, under-cured. |
| RSS4 | Dry mould no more than 20%, clean , dry, strong, small-scattered bubbles, specks of bark, free from blemishes, sand, foreign matter. |
| RSS5 | Dry mould no more than 30%, clean , dry, strong, large bark particles bubbles,small blisters, blemishes, free from sand, foreign matter. |